2016 GB/T and ASTM D Standard Stainless Steel Sagging Tester

Product Details
Customization: Available
Certification: GB/T 9264 and ASTM D 3730.
Overall Dimension: L120 * W20 * H20mm
Gold Member Since 2016

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

to see all verified strength labels (13)
Find Similar Products

Basic Info.

Model NO.
BGD225
Material
Corrosion Resistant Stainless Steel
Width of Wet Film
6mm
Space of Each Film
1.5mm
Suitable Industries
Wet Film Test Such as Paints, Printing Ink, etc...
Usage
to Determine The Relative Sag Resistance of Paint
Transport Package
Carton Box
Trademark
Glorythai
Origin
China
HS Code
9027809900
Production Capacity
3000 PCS / Month

Product Description


        BGD 225 Sagging Tester produced by our company is in accordance with the specification of
GB/T 9264 and ASTM D 3730. They are made of corrosion resistant stainless steel, the width of application is 75mm at 6mm per sagging thickness, and the gaps are being separated by a 1mm space as a marking on each sagging for distinctive identification of each sagging. 
        They are applicable to determine the relative sag resistance of a series of paints in order to provide the technical parameters for the paint application on site.
  

Main Technical Parameters

Clearance ranges:

Ordering information

BGD 225/1

BGD 225/2

BGD 225/3

BGD 225/4

BGD 225/5

RANGE

50-275μm

250-475μm

450-675μm

650-875μm

850-1,075μm


Difference between adjacent two notches: 25μm
Overall dimension:120×20×20mm(length by width by height)
The applicator can scrape 10 pcs of Parallel to the wet film in different thickness, the width of wet film is 6mm, space of each film is 1.5mm, thickness difference between adjacent film is 25μm
Weight: 0.5Kg
 

Manual:
Drawdown the coatings on a material(glass, test chart or board)using the appropriates sagging Thickness  Gauges, then place the coated material at vertical position(90º)to the platform(eg: table).Allow 10 to 30 minutes(depending on the viscosity)for the coatings to sag under gravity. Check out the coating thickness without the sagging effect and the next coating thickness with the sagging effect. With that information, the recommended coating thickness is between the 2 layers of coatings.
 


Please feel free to contact us  ↓↓↓  

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now
Contact Supplier